Impact of Various Desensitizing Agents on the Micro-Tensile Bond Strength of Adhesive Systems: In-Vitro Study

Jump To References Section

Authors

  • Armed Forces Dental Clinic, KG Marg, New Delhi - 110001, Delhi ,IN
  • Maulana Azad Institute of Dental Sciences, New Delhi - 110002, Delhi ,IN
  • Department of Conservative Dentistry and Endodontics, Maulana Azad Institute of Dental Sciences, New Delhi - 110002, Delhi ,IN
  • Department of Conservative Dentistry and Endodontics, Maulana Azad Institute of Dental Sciences, New Delhi - 110002, Delhi ,IN

DOI:

https://doi.org/10.18311/jpfa/2023/34096

Keywords:

Bond Strength, Composite Resin, Desensitizing Agents

Abstract

Objectives: To assess the influence of various desensitizing agents on the micro-tensile bond strength of various adhesive systems. Methods: Fifty extracted human permanent third molars, were sectioned at the cementoenamel junction in order to expose the mid-coronal dentinal tubules in parallel to the occlusal surface using a diamond disc and water coolant. The samples were divided into five groups and each sample was immersed in the respective desensitizing agent (Groups 1 to 5; Group 1- Distilled water, Group 2- Arginine calcium carbonate (Sensitive Pro-Relief Colgate- Palmolive, India, Group 3- Calcium sodium phosphosilicate (Repair and Protect, GlaxoSmithKline, India), Group 4- Strontium chloride hexahydrate 10% w/w (ICPA Health Products Ltd, India.), Group 5- Er,Cr: YSGG (Waterlase MD, Biolase, Irvine, CA, USA) with each group having a sample of n = 10. Each group was further divided into two subgroups (n = 5) based on the adhesive system (either a One-step self-etch adhesive (Xeno v+) (SE) or a two-step etch and rinse adhesive (Prime and Bond NT) (EandR)). Instron Micro tensile Tester was used to analyze the Micro-Tensile Bond Strength (MTBS) of the samples. Results: The bond strength of the control group (Group 1) was greater as compared to the other four groups, though statistically insignificant. There was a significant difference in the bond strength of the two subgroups (p<0.001) One-step self-etch adhesive (SE, Xeno V+) and two-step etch and rinse adhesive (EandR; Prime and Bond NT) adhesive. Conclusion: The use of desensitizing agents does not affect the micro tensile bond strength of adhesives used for the management of restoration of Non-Cervical Carious Lesions (NCCL). Microtensile bond strength with a self-etch adhesive system was significantly lower in the desensitized dentin irrespective of the agents used.

Published

2023-12-05

How to Cite

Rathod, A. A., Yadav, S., Nawal, R. R., & Talwar, S. (2023). Impact of Various Desensitizing Agents on the Micro-Tensile Bond Strength of Adhesive Systems: <i>In-Vitro</i> Study. Journal of Pierre Fauchard Academy (India Section), 37(3-4), 43–48. https://doi.org/10.18311/jpfa/2023/34096

Issue

Section

Original Research Article

 

References

Brannstrom M, Linden LA, Arstrom A. The hydrodynamics of dental tubule and pulp fluid. A discussion of its significance in relation to dental sensitivity. Caries Res. 1967; 1:10–7. https://doi.org/10.1159/000259530

Rees JS. The prevalence of dentine hypersensitivity in general dental practice in the UK. J Clin Periodontol. 2000; 27:860– 5. https://doi.org/10.1034/j.1600-051x.2000.027011860.x

Fischer C, Fischer RG, Wennberg A. Prevalence and distribution of cervical dentine hypersensitivity in a population in Rio de Janeiro, Brazil. J Dent. 1992; 20:272–6. https://doi.org/10.1016/0300-5712(92)90043-C

Gillam DG, Seo HS, Bulman JS, Newman HN. Perceptions of dentine hypersensitivity in a general practice population. J Oral Rehabil. 1999; 26:710–4. https://doi.org/10.1046/ j.1365-2842.1999.00436.x

Tuncer D, Yazici AR, Özgünaltay G, Dayangac B. Clinical evaluation of different adhesives used in the restoration of non-carious cervical lesions: 24-month results. Aust Dent J. 2013; 58:94-100. https://doi.org/10.1111/adj.12028

Arrais CAG, Chan DCN, Giannini M. Effects of desensitizing agents on dentinal tubule occlusion. J Appl Oral Sci. 2004; 12:144-8. https://doi.org/10.1590/S1678- 77572004 000200012

Cummins D. Recent advances in dentin hypersensitivity: Clinically proven treatments for instant and lasting sensitivity relief. Am J Dent. 2010; 23:3-13. https://doi. org/10.4103/0972-0707.73385

Walters PA. Dentinal hypersensitivity: A review. J Contemp Dent Pract. 2005; 6:107-17. https://doi.org/10.5005/jcdp-6- 2-107

Wara-Aswapati N, Krongnawakul D, Jiraviboon D, Adulyanon S, Karimbux N, Pitiphat W. The effect of a new toothpaste containing potassium nitrate and triclosan on gingival health, plaque formation and dentine hypersensitivity. J Clin Periodontol. 2005; 32:53–8. https:// doi.org/10.1111/j.1600-051X.2004.00631.x

Poulsen S, Errboe M, Lescay Mevil Y, Glenny AM. Potassium containing toothpaste for dentine hypersensitivity. Cochrane Database Syst Rev. 2006; 3:CD001476. https:// doi.org/10.1002/14651858.CD001476.pub2

Dragolich WE, Pashley DH, Brennan WA, Robert BO, Horner JA, Van Dyke TE. An in vitro study of dentinal tubules occlusion by ferric oxalate. J Periodontol. 1993; 64:1045–51. https://doi.org/10.1902/jop.1993.64.11.1045

Gillam DG, Mordan NJ, Sinodinou AD, Tang JY, Knowles JC. The effects of oxalate-containing products on the exposed dentine surface: and SEM investigation. J Oral Rehabil. 2001; 28:1037–44. https://doi.org/10.1046/j.1365- 2842.2001.00775.x

Pearce NX, Addy M, Newcombe RG. Dentine hypersensitivity: A clinical trial to compare 2 strontium desensitizing toothpastes with a conventional fluoride toothpaste. J Periodontol. 1994; 65:113–9. https://doi. org/10.1902/jop.1994.65.2.113

Chesters R, Kaufman HW, Wolff MS, Huntington E, Kleinberg I. Use of multiple sensitivity measurements and logit statistical analysis to assess the effectiveness of a potassium-citrate-containing dentifrice in reducing dentinal hypersensitivity. J Clin Periodontol. 1992; 19:256– 61. https://doi.org/10.1111/j.1600-051X.1992.tb00463.x

Petrou I, Heu R, Stranick M, Lavender S, Zaidel L, Cummins D, Sullivan RJ, Hsueh C, Gimzewski JK. A breakthrough therapy for dentine hypersensitivity: How dental products containing 8% arginine and calcium carbonate work to deliver effective relief for sensitive teeth. J Clin Dent. 2009; 20:23–31.

Pashley DH, Carvalho RM, Pereira JC, Villanueva R, Tay FR. The use of oxalate to reduce dentin permeability under adhesive restorations. Am J Dent. 2001; 14:89-94

Silva e Souza Jr MH, Carneiro KG, Lobato MF, Silva e Souza P de A, de Góes MF. Adhesive systems: Important aspects related to their composition and clinical use. J Appl Oral Sci. 2010; 18:207-14. https://doi.org/10.1590/S1678- 77572010000300002

Pereira PN, Okuda M, Sano H, Yoshikawa T, Burrow MF, Tagami J. Effect of intrinsic wetness and regional difference on dentin bond strength. Dent Mater. 1999; 15:46-53. https://doi.org/10.1016/S0109-5641(99)00013-5

Awang RAR, Masudi SM, Mohd Nor WZW. Effect of desensitizing agent on shear bond strength of an adhesive system. Arch Orofac Sci. 2007; 2:32-5.

Pashley DH, Carvalho RM, Sano H, Nakajima M, Yoshiyama M, Shono Y, Fernandes CA, Tay F. The microtensile bond test: A review. J Adhes Dent. 1999; 1:299-309.

Armstrong SR, Geradeli S, Maia R, Raposo LHA, Soares CJ, Yamagawa J. Adhesion in dentistry – analyzing bond strength test methods, variables and outcomes. Adhesion to tooth structure: A critical review of “micro” test methods. Academy of Dental Materials Annual Meeting – Portland, Oregon, USA. 2009; 29-31.

Inoue S, Vargas MA, Abe Y, Yoshida Y, Lambrechts P, Vanherle G, Sano H, Van Meerbeek B. Microtensile bond strength of eleven contemporary adhesives to dentin. J Adhes Dent. 2001; 3:237-45.

Wanga Z, Sa Y, Sauro S, Chen H, Xing W, Maa X, Jiang T, Wanga Y. Effect of desensitizing toothpastes on dentinal tubule occlusion: A dentine permeability measurement and SEM in vitro study. J Dent. 2010; 38:400-10. https://doi. org/10.1016/j.jdent.2010.01.007

Banomyong D, Kanchanasantikul P, Wong RH. Effects of casein phosphopeptide-amorphous calcium phosphate remineralizing paste and 8% arginine desensitizing paste on dentin permeability. Journal of Investigative and Clinical Dentistry. 2013; 4:200–6. https://doi.org/10.1111/j.2041- 1626.2012.00144.x

Cavalcanti AN, de Souza ES, dos Santos Lopes G, de Freitas AP, de Araújo RPC, Mathias P. Effect of a desensitizing dentifrice on the bond strength of different adhesive systems. Braz J Oral Sci. 2013; 12. https://doi.org/10.1590/ S1677-32252013000200015

Yang H, Pei D, Chen Z, Lei J, Zhou L, Huang C. Effects of the application sequence of calcium-containing desensitising pastes during etch-and-rinse adhesive restoration. J Dent. 2014; 42:1115-23. https://doi.org/10.1016/j.jdent.2014.03.018

Tuncer D, Yazici AR, Özgünaltay G, Dayangac B. Clinical evaluation of different adhesives used in the restoration of non-carious cervical lesions: 24-month results. Aust Dent J. 2013; 58:94-100. https://doi.org/10.1111/adj.12028

Aranha ACC, Siqueira Junior CADS, Cavalcante LMA, Pimenta LAF, Marchi GM. Microtensile bond strengths of composite to dentin treated with desensitizer products. J Adhes Dent. 2006; 8:85-90.

Shirai K, De Munck J, Yoshida Y, Inoue S, Lambrechts P, Suzuki K, et al. Effect of cavity configuration and aging on the bonding effectiveness of six adhesives to dentin. Dentet al Mater J. 2005; 21:110-24. https://doi.org/10.1016/j. dental.2004.01.003